Now Loading...

閉じる

Shipping Schedule

Shipping takes place on 10:00 a.m. ~ 19:00 p.m. business days.
Shipping is not available on weekends and holidays.

Same Day Delivery

Same day delivery is available for orders submitted before 12:00 noon, payments by credit card, and with all items in stock.
Excluding weekends and holidays.

ギフトラッピングについて

全ての商品はギフトラッピングが可能です。「ギフト」画面からギフトラッピングを商品と一緒にご注文ください。

※セット数や受注状況により発送までに多少お時間をいただく場合があります。お急ぎの場合はご相談ください。

Prendre saucer

studio m'

  • ¥1,320 (Including tax)
    

Product Information

Size

φ:直径 / W:幅 / D:奥行 / H:高さ / L:長さ

( )の数字は有効寸法です。

※多少の誤差が生じます。

容量:

※多少の誤差が生じます。

○内容量表示は、満水の状態で計測しています。

○ポットの場合は水平に置いてこぼれない容量です。

○内容量表示は、概ねの目安として下さい。

Features
  • Color Shade Variations
  • Color Shade Variations

    Each piece has individual color shade variations. Affected by glazes and natural firing conditions such as changes in temperature, humidity and other climate elements and also how to receive the fire in the kiln chamber, each piece has own expression. It is really difficult to make the completed ware exactly same in color by firing and glazing even when the same materials are used. 100 pieces show 100 kinds of expressions, as it were.

  • Color Irregularities
  • Color Irregularities

    There are color irregularities of applying a glaze or slip, which are different from part to part in a piece of ware. For example, some parts are glazed thinly or thickly depending on the shape of the ware. That leads to part-to-part subtle differences in appearance of the clay in a piece of ware.

  • Glaze or Slip Drips
  • Glaze or Slip Drips

    The glaze or slip may look like dripping. There is unevenness of a glaze or slip when they are applied to ware by hand. There also appear glaze drips or slip drips, which are caused by the glaze or slip flows during firing.

  • Pinholes
  • Pinholes

    Pinholes may be seen clearly on the surface. Pottery (earthenware) is mainly made from earth, and green ware contains a lot of air while biscuit firing. While glazed firing, this air inside the biscuit ware becomes air bubbles, which remain and look like small holes on the surface of the glazed part. Those small holes are called pinholes.

  • Crazing (Chaps)
  • Crazing (Chaps)

    Crazing (having chaps) may appear clearly on the glazed part. The “direct” crazing means having chaps originally. The “aging” crazing means having chaps over time as you use the tableware item. There is a difference between the shrinkage rate of the glaze and that of the clay, so crazing occurs. Note that those cracks do not come from the damage of tableware items. They might appear just before use, but it is no problem in terms of use. They appear on the surface of pottery (earthenware) and semi-porcelain.

  • Iron in Powder
  • Iron in Powder

    Iron in powder may be seen clearly on the surface. Pottery (earthenware) is made from earth, which contains iron. After firing green ware, iron appears on the surface in the form of black dots. Red or black earthen clay contains much more iron, and as a result, not a little iron in powder may appear on the surface of tableware items made from this type of clay.

Materials (Number)

Ceramics are handled differently depending on the material. MARUMITSU POTERIE attaches a material number sticker to ceramic products. Please note the material number when handling the product in order to ensure long use.

Pottery

Features

・Seasoning earthenware before use and for the first few times are essential to protect from stains and soiling. Please refer to “How to season earthenware”.
・Do not use abrasive cleansers and metal scrubbing brushes for items with over glazed designs and decorations. It may cause damage to the over glaze.
・There are products with a crackle effect on the surface as an intended design, and there are some products that will develop crazing over time.
・Following features may be seen in some products which is derived by its material and manufacturing process.

Before using the item

・Before each use, soak in a sufficient amount of clean water and let it absorb for at least 30 minutes. This will block moisture from food and helps to prevent or reduce stains, mold and mildews. Visible spots may appear after this procedure, showing the item has absorbed water. The spots will disappear as it dries.

After use

・Even after seasoning, boiled extracts and oils will be gradually absorbed due to the porous nature of earthenwares. Wash immediately after each use and let it dry completely before storing to prevent odor, stains, mold and mildews.

マテリアルナンバー一覧

  • Pottery

made in POTTERY

CODE
102783

Items in the same series

Look-Alike